GC Solar 23.61 GW GD Solar 53.65 GW
Technical Article

Galvanic corrosion in metal structures of photovoltaic systems

Understand what galvanic corrosion is and the impacts of this process

Galvanic corrosion in metal structures of photovoltaic systems

There are measures that can be adopted to prevent galvanic corrosion of metal structures

Photovoltaic systems have a long projected lifespan, typically 25 years. To ensure the longevity of the project, we must study and guarantee the durability of all individual components. One of the most critical components in terms of durability and safety is the mounting structure for the photovoltaic modules.

With varying shapes and applications, we can find them installed in many different ways, in various types of environments and exposed to different weather conditions. Structures can fail in several possible ways.

The main causes of defects are incorrect installation, negligence in sizing calculations (especially due to wind load), inappropriate choices of fixing method, excessive load on the structure and corrosion of the material.

Figure 1 – The module fixing solutions are very varied, each with a different characteristic from the point of view of bimetallic corrosion; (a) ceramic roof with aluminum support structures; (b) zinc-plated steel metal roof and steel structure; (c) ground structure with directly buried zinc-plated steel

This article aims to show what concerns the designer and installer should have when selecting a structure and the fixing method in relation to the material's durability and corrosion resistance.

Bimetallic corrosion or galvanic corrosion

We call galvanic corrosion the electrochemical process in which two metals in contact begin a corrosion process caused by the transfer of electrons in the presence of an electrolyte. All metallic alloys have an electrical characteristic associated with them, referring to the ease with which the metal gives up electrons to the environment in which it finds itself.

The ease of a metal in giving up electrons is called electropositivity, while the tendency to absorb electrons is called electronegativity. According to the nomenclature used in the field of chemistry, the material with greater electronegativity has a greater reduction potential.

It is also said that the more electropositive material has greater reactivity, that is, one material is more reactive than another (has a greater tendency to lose electrons) when it has greater electropositivity.

When a metal or metallic alloy comes into contact with another alloy with different electronegativity, an electrical potential appears between the two materials. With the addition of an electrolyte, which is an aqueous medium capable of conducting ions and electrons, a galvanic cell or battery is formed.

This is the same working principle as a common battery – two distinct metals separated by an electrolyte. The galvanic cell causes a current to flow from the most electropositive material (anode) to the most electronegative material (cathode).

The anodic metal alloy will suffer corrosion, since the process of donating electrons forms ions that can become detached from the metal. For example, an iron alloy acting as an anode undergoes the following chemical reaction:

Fe → Fe2+ + 2e

This reaction removes the iron from the metal alloy and makes it available in the form of iron ions to the electrolyte. The iron ion combines with oxygen in the air and causes rust (iron oxide II and III mainly). Meanwhile, at the cathode, the metal receives the electrons given up by the anode.

Figure 2: Simplified bimetallic corrosion scheme
Figure 2 – Simplified scheme of bimetallic corrosion

Galvanic corrosion occurs significantly when there is a difference in electronegativity of the alloys in contact greater than 0,5V. The table below shows the electronegativity values ​​relative to gold of the most common metallic alloys.

Table 1 – Electronegativity values ​​of common alloys in relation to gold

Table 1 - Electronegativity values ​​of common alloys relative to gold

Corrosion becomes more critical if the anode area is smaller than the cathode area. In this case, the anode gives up electrons to a much larger area and therefore has its degradation accelerated.

Figure 3 - The anode has a corrosion rate that depends on the area ratio between the anode and the cathode
Figure 3 – The anode has a corrosion rate that depends on the area ratio between the anode and the cathode
Figure 4 - Screw and nut suffering galvanic corrosion in a metal structure. Corrosion in screws is a concern as it can cause serious failures in the structure.
Figure 4 – Screw and nut suffering galvanic corrosion in a metal structure. Corrosion in screws is a concern as it can cause serious failures in the structure.

If a screw is in contact with another material that makes it an anode, it corrodes quickly, increasing the risk of breakage and loosening of the tightness. In short, for galvanic corrosion to occur, it is necessary that:

  1. There is an electrolyte connecting the two metals: the electrolyte in the case of structures exposed to the weather is water, air humidity and sea air;
  2. Electrical contact between the two metals: if there is an insulator between the two metals, there will be no path for the galvanic current to flow, therefore galvanic corrosion does not occur;
  3. A difference in electropositivity or electronegativity greater than 0,5 V.

Galvanic corrosion protection

There are measures that can be taken to prevent galvanic corrosion of metal structures. The first measure, which is not always possible, is to use metals that are compatible with each other, that is, that have an electronegativity difference of less than 0,5 V. It is not always possible to analyze in advance each combination of metal used in the structure to be assembled in the field at the client's site.

A second measure may be the selection of materials such that the anode has a much larger area than the cathode. When this occurs, corrosion is reduced and may become insignificant, depending on the relationship between the areas and the absence of electrolyte (in regions with a dry climate, with little humidity in the air).

If it is not possible to choose compatible materials, one solution is to ensure that the metal parts of a structure have some treatment that prevents galvanic corrosion. This treatment can be adding a layer of zinc to the steel, anodizing the aluminum or carrying out special surface treatments.

The zinc layer on galvanized steel or galvanized steel protects the steel from contact with oxygen and other external sources of corrosion. Zinc also acts as a sacrificial anode if this barrier is broken, giving electrons to the steel and preventing it from disintegrating.

Figure 6 - A very common application of galvanized steel can be found in metal tiles. Galvanizing protects steel from the elements and minimizes the effects of galvanic corrosion
Figure 5 – A very common application of galvanized steel can be found in metal tiles. Galvanizing protects steel from the elements and minimizes the effects of galvanic corrosion

The installation location is a determining factor in the durability of galvanized structures. The installation location directly influences the thickness of the zinc coating to be applied. The zinc coating corrodes over time and can expose the steel to corrosion if the correct thickness is not observed. The corrosion rate of the zinc coating depends directly on the environment in which it is located and the metal it protects, as shown in the table below.

Table 2 – Estimated corrosion of the zinc protective layer for each type of metal in contact and installation environment, in micrometers per year

Table 2 - Estimated corrosion of the zinc protective layer for each type of metal in contact and installation environment, in micrometers per year.

In coastal or oceanic regions, the problem of metal corrosion is accentuated due to the salinity and high humidity of the environment, two aspects that favor the formation of electrolytes in metallic structures.

In the figure below, we see an example of corrosion accentuated by sea spray in a coastal location. The photograph specifically shows a case of bimetallic corrosion due to the contact of grounding terminals with the frame of the photovoltaic module.

Typically, these connectors are made of copper, bronze (tin and copper alloy) or brass (copper and zinc alloy), which have greater electronegativity than aluminum. Being more electropositive, aluminum tends to disintegrate.

Figure 7 - The fixing mechanism between the copper wire and the module contained incompatible metals. The degradation process was accelerated by sea air
Figure 6 – The fixing mechanism between the copper wire and the module contained incompatible metals. The degradation process was accelerated by sea air

In some cases, it is possible to carry out other types of surface treatments or adopt strategies to isolate incompatible metal parts. If the metals are isolated from each other or isolated from the electrolyte, there is no longer any way for the anode to give up electrons to the cathode.

This insulation can be chemical (with the surface treatment of the parts) or physical (where the metallic parts are separated by an insulator). The physical solution is not always viable, as it may represent an increase in the cost of the work and the need for more frequent maintenance in order to check the quality of the insulation.

Aluminum alloys can be protected by growing an additional layer of oxide on their surface. The oxide that is formed acts as an electrical insulator, thus reducing current flow and bimetallic corrosion when in contact with another alloy.

Aluminum treated in this way is called anodized aluminum. Because of its good durability and compatibility, anodized aluminum is the most common material in the construction of photovoltaic module frames and fixing structures. 

Despite its advantages, aluminum is expensive and can be successfully replaced in some cases by steel. subjected to anti-corrosive surface treatments such as galvanizing, phosphating and electrophoretic painting.

The protective layer created by surface treatments must prevent material contact due to the presence of electrolyte, typically formed by condensate, dust, dew, rain, wet residues in contact with metals, soil moisture and others.

With the isolation between metals, the galvanic cell is not formed, thus interrupting the exchange of electrons, generation of ions and galvanic corrosion. An important point in the treatments on structures for photovoltaic systems is UV (ultraviolet) protection compatible with the other components.

The structures are exposed and therefore subject to an important risk factor in defining the corrosion protection used. The most common surface treatments found in the industry and which can also be applied in the photovoltaic segment, in addition to traditional galvanization, are phosphating and cathodic electrophoresis.

Phosphating is a surface treatment widely used in the automobile industry, which offers good anti-corrosion protection and good adhesion to paintwork. Phosphating is normally used as preparation for a final surface treatment, as is the case with cathodic electrophoresis (KTL), which adds a film of organic pigments and gives metal parts extraordinary protection against corrosion.

Corrosion in soil structures and grounding systems

All solar systems require grounding. In systems implemented on the ground, the metal of the structure and the grounding grid are buried, which are typically made of different metals and can corrode each other.

The grounding grid is typically made of bare copper buried directly into the ground and the buried metal structure is typically aluminum or steel. Both metals in the structure form galvanic batteries with copper, however the relationship between the areas of the metals is such that the corrosion caused by the association is small.

For additional fixation and durability purposes, alloy steels are commonly attached to buried concrete footings. Concrete forms a kind of film on the steel that reduces the effects of galvanic corrosion on the material.

This does not eliminate the concern about galvanic corrosion, as connections to the grounding system must still be made with compatible metals. Materials can also suffer other corrosion processes related to the acidity and composition of the soil.

Corrosion in photovoltaic systems

The designer and installer must be careful when selecting the structure for a photovoltaic system. Corrosion of structures in these systems occurs mainly due to:

  • Incompatibility between the metals of the structure, module and roof;
  • Choosing incompatible screws. For example, zinc-plated steel screw in stainless steel structure;
  • Damage to the anodizing layer of aluminum or galvanized steel;
  • Metals unsuitable for locations with significant salt air.

Conclusion

The appropriate choice of materials for the construction of fixing structures is an important factor in determining the useful life of photovoltaic systems. Screws, grounding clips and structural parts must be chosen according to the electronegativity of each material.

The installation environment must also be taken into account. Oceanic regions, with the strong presence of salinity, can present accelerated corrosion of materials. In all cases, it is important to check the type of treatment used by structure manufacturers, such as the KTL process (cathodic electrophoresis), the Geomet process and others.

Matthew Vinturini
About the Author
Matthew Vinturini

Specialist in photovoltaic systems and electrical engineer graduated from UNICAMP (State University of Campinas). Science and technology enthusiast, with experience in the field of solar energy, both commercially and in the design, dimensioning and installation of photovoltaic systems. 

Comments (1)

Comments are moderated before publication.

Comments should be respectful and contribute to a healthy debate. Offensive comments may be removed. The opinions expressed here are those of the authors and do not necessarily reflect the views of the author. Canal Solar.

Leave your comment

  • Multi

    Galvanic corrosion occurs in metal structures when dissimilar metals come into contact with each other in an environment containing electrolytes, such as water or moisture, creating an electric current that accelerates corrosion. This type of corrosion is common in solar energy structures and other metal installations exposed to the environment. To prevent it, it is essential to use compatible materials, adopt protective coatings and electrically isolate the metals in contact.

Canal Solar
Privacy

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognizing you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.